Common problems and solutions in the production process of BOPP film

Common problems and solutions in the production process of BOPP film
As a professional BOPP film supplier, CHALVO has a lot of detailed cases to share to all, and hope it can help the production partners.
The main goals to be achieved in the BOPP film production process are, first and foremost, to achieve continuous production at the highest possible speed, followed by improving the performance of the BOPP film, ensuring quality, and reducing energy consumption.
However, in the actual production process, due to various reasons, various problems arise with BOPP film, making it difficult to achieve production goals. The author proposes solutions to common production problems based on the 8.2m BOPP film production line from French company DMT.
1.Horizontal stripes
Large-gap horizontal stripes are mainly caused by unstable extrusion melt pressure, uneven rapid cooling roll speed or temperature, or excessive fluctuations in wind knife airflow.
The most common cause is that the production line speed increases too fast, causing the metering pump to increase rapidly, while the main extruder screw speed increases relatively slowly, resulting in insufficient head material output and unstable pressure. When encountering this situation, the best solution is to extend the acceleration time appropriately until the line speed stabilizes and the horizontal stripe disappears naturally. Another common cause is material factors. If all process conditions are well controlled and there is no significant improvement after multiple adjustments, it is necessary to consider replacing the material. Small-gap horizontal stripes are not common in actual production and are caused by unsuitable angles of the machine head, wind knife, or nearby airflow, or unstable roll speed.
2.Vertical stripes
During the casting process, continuous vertical stripes may appear in the extruded cast at specific locations, which can cause uneven thickness of the BOPP film and obvious bumps or vertical stripes in the appearance of the rolled and cut film. To eliminate vertical stripes, it is necessary to use a well-designed and high-quality die with a smooth outlet and no mechanical damage, strengthen melt filtration, promptly clear debris from the outlet, maintain the die head, improve the uniformity of air-knife blowing, control the temperature of each extrusion section reasonably, and adjust the position of the die head relative to the cooling roll.
3.Bending on both sides
This phenomenon is mainly caused by poor attachment effect and too large temperature difference between both sides during casting. Bending may affect the flatness of the film. For PP, because the casting cools unevenly, the crystallization is uneven, directly affecting the film-forming properties of the film. Usually, the casting edges are bent towards the lower temperature side, so the temperature of the cooling water in the cooling tank and the rapid cooling roll surface can be judged based on the casting bending condition during the production process and then addressed.
4.Bubbles
If impurities are carried in the melt, the raw material contains excessive moisture, the extrusion temperature is too high, the material heating time is too long, or air or degraded substances accumulate in the extruder or filter, bubbles may appear in the cast. If bubbles appear during normal production, the shape and color of the bubbles should be carefully observed, the cause analyzed, and a solution found. If there is air or degraded materials in the extruder or filter during the initial extrusion or when replacing the new melt filter and restarting the extruder, bubbles will generally occur in the casting, and this problem can usually be solved by sufficient discharge.
5.Irregular edges
The irregular edges of the casting may be caused by damage to the sealing elements at both ends of the die lip, abnormal edge-pressing system, or unstable melt extrusion pressure. After identifying the cause, the corresponding method should be used promptly to resolve it, or horizontal stripping may occur.
6.Other defects
Other casting defects may occur during the casting process, such as crystal points, coke, unmelted materials, unsuitable crystallinity and glossiness, or sharkskin. These defects generally do not occur in production lines with mature processes and high technical levels.
CHALVO is a company that specialises in customised packaging solutions as well as production. Feel free to send us any content on packaging, progress and growth together will be our constant theme.